Kun jumɛn de bɛ kɛ ka ɲɛgɛnɛsiraw dilan die casting machine yɔrɔw la minnu bɛ yɔrɔ kelen na?

Nov 03, 2021

Walasa ka die-casting masin baaracogo ɲuman sabati, dɔnniya ladonni ka kan ka kɛ k’a sɔrɔ a bɛ baara kɛ ni a ye ka ɲɛ. Mun bɛ kɛ sababu ye ka ɲɛgɛnɛsiraw dilanni kɛ die casting machine yɔrɔ fitininw na?


1. Kɔnɔna da teliya ka bon kojugu, lamaga-lamagali bɛ tɛmɛ, wa nɛgɛ bɔli sen bɛ gazi la kosɛbɛ.


2. Kɔnɔna da la, a yɔrɔ tigɛlen ka dɔgɔ kojugu ani pikiri in ka jugu.


3. Kɔnɔna da jɔyɔrɔ tɛ hakili la. kɔnɔna da la, nɛgɛ bɛ kogo cogoya la yɔrɔnin kelen ani ka vortex bɔ, ani gazi bɛ nɛgɛ jibɔ la.


4. Ɲɛgɛnɛsiraw jɔyɔrɔ ka jugu ani tigɛyɔrɔ tɛ se ka kɛ, o bɛ na ni sɔgɔli cogoya jugu ye.


5. Masina belebele die-casting yɔrɔ misɛnninw, degun so fa ka dɔgɔ kojugu, kɛrɛnkɛrɛnnenya la Horizontal Die Casting Machine. kan.


6. casting dilanni ye hakilintan ye: casting yɔrɔ minnu sɛgɛn ka gɛlɛn; b Sigida yɔrɔ kogo janya ka bon kojugu.


7. Surface ka baarakɛcogo hakɛ min bɛna baara kɛ, o ka bon kojugu, o bɛ kogo janya bonya kojugu.


8. Nɛgɛ wulilen bɛ gazi caman sɔrɔ.


The pores of the semi-solid parts of the die-casting machine are divided into two types. One is the holes with bright and smooth inner surface formed by the metal involved in the gas when filling. The other is that the alloy smelting is incorrect or insufficient, and the gas is melted into the alloy. During die-casting, the chilling is very dramatic, and the solidification is very Fast. Gazi min bɛ wuli nɛgɛ kɔnɔ, o bɛ tɛmɛn ka tɛmɛ, fo nɛgɛ min bɛ nɛgɛ la, o bɛ to bɔgɔ la ani ka dingɛw dilan. porow minnu bɛ die-casting masin tilayɔrɔbaw la, olu ye gazi ye min bɛ sɔrɔ nɛgɛ kɔnɔ, ani gazi fanba ye fiɲɛ ye.